全部| 技术文章| 新品上市| 最新资讯| 行业聚焦| 案例故事| 图片|
;
工程机械之家>文章分析>Vogele paver "on the heat" paving layer
Vogele paver "on the heat" paving layer
来自:工程机械之家 时间:2014-06-11 浏览数:0

Vogele paver "on the heat" paving layer joint introduction       

"Hot to hot" paving layer refers to two or more than two paver at the same time before and after paving, the final roller compaction of the entire paving.

Car should be arranged, the feeding time, Taiwan paver at the same speed and the same distance. When the paving is finished, the temperature of the paving layer should be approximately the same, so as to ensure the compaction effect is consistent.

Paver should be the best use of the same type of screed, and set the same, so as to maintain consistent pre compaction effect.

Be careful:

The compaction between the joints shall take into account the final compaction of the rollers. Otherwise, the roughness of the cross slope will be affected, and the area of the road will also be affected.



上一篇: 下一篇: