Vogele paver surface structure repair mixture solution phenomenon

error

Sporadic bulk segregation will block the paving process. The paving surface smooth or asphalt oil.

Reason

Paving material and high content of asphalt aggregate too small. May be due to the residual asphalt mixing station mixing paving material.

This may be due to inadequate screed heating. In this case, the asphalt will be stuck with the hammer shield or hammer, change the paver structure.

Remedy method

Check the screed heating function is open and work.

The Paver Screed and at the end of the work should be thoroughly cleaned.

If necessary, should remove, clean and re adjust the rammer cover.

Notify the operator of the mixing station to segregate.

Reduce the speed of rammer.